TAG (thermogravimetric analysis)

The highlights

High Performance Symmetrical TGA System (ambient / 1750°C)

– Outstanding isothermal balance performance for long term corrosion/oxidation studies
– No buoyancy effect with dual furnace design for high precision DTA/DSC
– Unique sample geometry for near 100% surface area studies
– Mass Spectrometry Coupling
– Calisto software

The TAG system is the world’s most precise isothermal TGA system. It features the same symmetrical balance beam and aggressive atmosphere control seen in the SETSYS system. In addition it incorporates a pair of matched furnaces which eliminates buoyancy effects and provide unparalleled performance. If you are studying long term corrosion and / or oxidation then nothing comes close to the TAG’s performance.

Specifications
Temperature Range Ambient to 1600°C or 1750°C
Programmable temperature scanning rate (heating and cooling) 0.01 to 100°C
Balance Capacity 35g
Gases 3 carriers gases (MFC from 4 to 200 ml/min) + 1 auxiliary or reactive gas (MFC from 0.3 to 16 ml/min)
Crucibles From 55 to 1500 μl – Alumina, Tungsten, Graphite, Platinum, Quartz, Aluminium
Rods TGA, DTA and DSC interchangeable rods
Weight 145kg (320 lbs)
Dimensions (Height / Width / Depth) 170 / 60 / 55 cm (66.9 / 23.6 / 21.6 in)
Power Requirements 230V – 50/60Hz
Features

With its wide temperature range (from ambient up to 1750°C) the TAG has a large range of applications, especially in the field of advanced materials (ceramics, metals, alloys, inorganic compounds, oxides, nanotubes) to investigate phase diagram, long term thermal stability, corrosion, oxidation/reduction,adsorption, etc., under dry, humid or corrosive atmospheres.

Documentation


Brochures
Application notes

This is an extract of our documentation, please register to have access to all documentation



Simultaneous Thermogravimetry & Differential Scanning Calorimetry / Differential Thermal Analysis (STA, TGA-DTA/DSC) : TAG par SETARAM