96 Line TGA (Thermogravimetric Analysis)

The highlights

Large volume & high temperature Thermogravimetric Analyzer TGA (ambient to 2000°C)

This is an extremely high performance weighing module used with the TGA 96. This balance can weigh samples up to 100 g and is well suited to measuring both micro-quantities of samples (a few milligrams) as well as large, dense samples, while maintaining measurement resolution to within a microgram whatever the mass analyzed.
Several configurations are possible to analyze samples with the TGA 96:
– sample placed in a crucible directly suspended from the balance (several types of crucible available);
– sample suspended directly from the balance without being placed in a crucible beforehand (maximum sample dimensions: length 80mm, height 20 mm);
– sample placed in a TGA rod with built-in thermocouple in order to measure its temperature.
Simultaneous TGA-DTA/DSC measurements are also available.

NEW PARTS AND OPTIONS
Pierced alumina crucibles
Alumina based crucibles pierced with numerous orifices to improve sample / gas interactions are available. 18mL and 4.5mL versions are available.

FTIR coupling
A heated MS or FTIR 200°C coupling was designed for the TG96 line.

Specifications
96 Line TGA
Temperature range of measurement module(C°) amb/1600, amb/1750, amb/2000
Volume of crucible (μl) 18000
Max. sample size(mm) n/a
Resolution 0.3 μg
RMS noise 0,3 μg
Specific RMS noise 0,016μg/ml
Measurement range +/- 2000 mg
Features

Simultaneous TGA-DTA
– Ambient to 1600°C,
– Ambient to 1750°C,
– Ambient to 2000°C.
Simultaneous TGA-DSC
– Ambient to 1500°C,
– Ambient to 1600°C.