The highlights

Horizontal dilatometer (room temperature / 1200°C)

 

The HIGHLIGHTS:

C-Therm dilatometers offer high resolution and stability across a broad measurement range. With unparalleled ease-of-use, high adaptability, and modular design, C-Therm dilatometers offer researchers a robust cost-effective solution to their characterization needs.

 

See also: SETSYS Evolution TMA, TCi

Specifications
Temperature Range Room Temperature to 1200°C
Temperature Resolution 0.1°C
Max Displacement 4mm
Change of Length Resolution 1.25nm/digit
Atmosphere Air, Vacuum, Inert Gas
Sample Dimensions 10 to 50mm long x max diam. 12mm
Sample Holder Fused Silica, Alumina
Configurations Single or Dual LVDT System
Heating Element Kanthal wire (FeCrAl)
Rate of Increase Up to 50°C/min
Features

Furnace
The horizontal configuration provides users flexibility in sample placement and geometry making it easy and versatile solution.
Samples
The C-Therm dilatometer can offer sample formats up to 50mm in length.  Additionally, the system can offer a dual-sample configuration in doubling the testing capacity or be run as a differential measurement.
Electronics & software
C-Therm’s dilatometer was developed with the same central controller as C-Therm’s TCi Thermal Conductivity Analyzer – offering clients savings of up to 40% in combining the two!
C-Therm’s dilatometer uses its own data acquisition software and produces data files that are fully compatible and importable in the state-of-the-art Calisto data treatment software.

Applications

The C-Therm dilatometer provides unparalleled ease of use in the study of bulk polymers, ceramics, glass and metal alloys.

videos
The All-New TCi Thermal Conductivity Analyzer (with optional dilatometer)
High Precision Dilatometer from C-Therm Technologies

C-Therm dilatometers offer high resolution and stability across a broad measurement range in the measurement of thermal expansion. With unparalleled ease-of-use, high adaptability, and modular design, C-Therm dilatometers offer researchers a robust cost-effective solution to their characterization needs.

Thermal Analysis : C-Therm Dilatometer par SETARAM