Calvet DC Alexsys

Heat and Heat Capacity measurements up to high temperatures.

A question? Contact Us!

Calvet product hero

For Capable and Highest Accuracy Drop Calorimetry

 

CALVET DC ALEXSYS uses a 3D sensor based on thermocouples’ networks, dedicated to the drop calorimetry method.

Drop calorimetry consists of letting a sample fall (at room temperature) into the sensor (at high temperature).

 

DOWNLOAD THE BROCHURE

Applications

Interested in the stability of metals, alloys, ceramics or minerals? You can enjoy drop calorimetry measurements: heat of formation, heat capacity, heat content. They help to predict materials’ reactivity and structure changes. They are also used in methods for calculation of phase diagrams (like CALPHAD).

Why is it Unique?

  • BEST IN CLASS HIGH TEMPERATURE MEASUREMENTS BY DROP CALORIMETRY

    improved heat capacity, heat of phase transitions, heat content measurements

  • HIGHLY SENSITIVE HIGH TEMPERATURE 3D SENSOR

    dual drop capability with a measurement drop tube and a reference drop tube

  • ISOTHERMAL CONDITIONS

    up to 800 or 1000 °C

  • FINE CONTROL OF THE SAMPLE REACTIVITY

    and preserved sensor lifetime with various protections and inerting options

Documentation

Access the most relevant documents about our solutions and their use.

Request a quote for Calvet DC Alexsys

    This website is protected by reCAPTCHA, and Google’s privacy policy and terms of use apply.

    Access premium documentation

    Benefit from detailed application information

    setaram-CTA