Fossil Energies

Description

fossilenergies-calorymetry

Fossil fuels are mainly used for their heat content through combustion. In a first step, it is needed to classify the different fossil fuels, especially in term of fixed carbon. Heat capacity has to be known in the industrial process. Pyrolysis of fossil fuels can also be industrially used. A good knowledge of the gases emitted during the thermal transformation is needed.

Classification: Due to the large rank of solid fuels, especially coal, a classification based on the composition of the sample is needed. For coal, a standard thermogravimetric determination gives the ratio of moisture, volatiles, fixed carbon and ash.

Characterization: Pyrolysis is a thermal transformation that is very common with fossil fuels. As it produces different types of gases, the combination between thermogravimetry (TGA) and evolved gas analysis (EGA) is very helpful for such an investigation.

Combustion: DSC and calorimetry are used to investigate the combustion of fossil fuels and measure the corresponding heat of combustion. As a stoechiometry in oxygen is needed in such a pressure, the sample has to be heated under an adequate pressure of oxygen.

Heat capacity: If the calorific value of fossil fuel is of first importance, the knowledge of the value of its heat capacity is also necessary to establish the heat balance for the thermal process.

Wax appearance temperature (WAT) is easily determined by low temperature DSC

 Some References
VEOLIA Environnement

Associated products

Controlled Humidity Generator

Wetsys

Wetsys

The WETSYS is a stand alone, simple and robust system designed to generate atmospheres with a controlled humidity level. HIGHLIGHTS include: Accurately controlled atmospheres with humidity levels up to 95% RH Operations with gases such as air, He, Ar, N2, CO2… A heated transfer line with a standard connection for coupling to...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG - DSC - coupling to gas analyzer

SENSYS-EVO-DSC-H-300dpi

SENSYS evo DSC

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG – DSC – coupling to gas analyzer   The HIGHLIGHTS Incomparable precision: the unique 3D sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you...

Read more »

An innovative line of Thermal Analyzers (-120 / 830°C) with 3D-Inside technology: DSC, High Pressure DSC, Robot DSC, TG-DSC-coupling to gas analyzer

SENSYS_evo_TG-DSC

SENSYS evo TG-DSC

The HIGHLIGHTS Differential Scanning Calorimeter – Incomparable precision: the unique 3D DSC sensor totally surrounds your sample and reference crucibles so that the entire energy of any transformation is monitored thereby giving you...

Read more »

High Temperature 3D Calvet Calorimeter (up to 800 / 1000°C)

AlexSys-Calorimeter

AlexSys

Sensitivity, stability, flexibility and precision: The AlexSys calorimeter features a 3D Calvet sensor, providing high sensitivity and exceptional precision. The calorimeter block and furnace design ensures a high signal-to-noise ratio,temperature and signal stability, and low detection limit permitting low energy and slow reactions to be...

Read more »

Large volume & high temperature simultaneous TGA & DSC / DTA (ambient to 2000°C)

96-LINE-TG-300dpi

96 Line TGA – DTA / DSC

This is an extremely high performance weighing module used with the TGA 96. This balance can weigh samples up to 100 g and is well suited to measuring both micro-quantities of samples (a few milligrams) as well as large, dense samples...

Read more »

Large-volume & high-temperature ThermoMechanical Analyzer TMA (ambient to 2000°C)

96-LINE-TG-300dpi

96 Line TMA

The TMA 96 has a vertical configuration that permits working under very low loads (from 2 g) without subjecting the sample to stress. The displacement sensor of the TMA 96 is both robust and highly accurate. It detects very low variations of displacement on large samples....

Read more »

Mastering High Pressure DSC & Microcalorimetry up to 1000 bars - 14,500 psi

HP microDSC

HP Micro DSC

Mastering High Pressure DSC & Microcalorimetry up to 1000 bars – 14,500 psi Originally designed under a IFP (Institut Français du Petrole) license to study the gas hydrates formation and dissociation, the high pressure version of the μDSC7 evo offers unique capabilities on the market: on a wide temperature range, from the subambient temperature of...

Read more »

Reaction, isothermal and scanning calorimeter (ambient to 300°C)

C80-300dpi

C80

Incomparable precision of measurement: the 3D Calvet sensor totally surrounds the sample, and all heat evolved is measured. Now matter how small or large the thermal transformation the system provides a complete picture of the event. Absolute calibration: with a three-dimensional transducer the sensitivity of the C80...

Read more »

High-performance modular DTA & DSC thermal analyzers (ambient / 2400°C)

SETSYS-Evolution-closed

SETSYS Evolution DTA/DSC

The HIGHLIGHTS SETSYS Evolution is the standard for high performance TGA, TG-DSC and TG-DTA application.  It is based on a complete modular thermal analysis platform for – TGA, DTA and DSC – Simultaneous TGA/DTA and TGA/DSC – Dilatometry / TMA The key to the SETSYS...

Read more »

An-easy-to-use Differential Scanning Calorimeter DSC (-170 to 700°C) with a 3-year warranty

DSC131-300dpi

DSC131 evo

The HIGHLIGHTS – Robustness: the DSC131 evo features a highly robust sensor that, if needed, can readily be changed by the user in less than 30 minutes. No other DSC offers such flexibility. – Ease of operation: dedicated market leading CALISTO software that...

Read more »

Documentation

Application notes
Articles See articles