This thermal analysis method uses MOLECULAR MOBILITY to access structural information that cannot be obtained by any other technique. It also gives access to dynamic parameters (ΔH, ΔS and relaxation time ζ).
Properties measured by TSC include polymorphism, crystalline/amorphous rate, purity, glass transition, relaxation phenomena, etc.