High Temperature Calvet Calorimeter (up to 800 / 1000°C)
![]() |
precision. The calorimeter block and furnace design ensures a high signal-to-noise ratio,temperature and signal stability, and low detection limit permitting low energy and slow reactions to be measured. The sensitivity of the AlexSys does not change by more than 2% with
- weight, shape and nature (powder, pellet, fiber, liquid, etc.) of sample,
- contact between sample and crucible,
- crucible material,
- sweeping gas (inert or oxidizing) and its flow rate.
The sample chamber is big enough (working volume 20-30 cc depending on
sample cells) to contain a variety of assemblies, to provide mixing and gas bubbling through the solvent, and to design experiments to simulate different thermochemical processes at high temperature.
Ease of operation: The leading CALISTO software provided with the calorimeter is intuitive and powerful, enabling any typical or special-design experiment and data analysis to be performed. The calorimeter operates isothermally, with temperature and sensitivity stable over many months.
Sample loading and handling is straightforward.
AlexSys sensor
Application Documents
|
See all application documents |
文献集
|
文献を見る |
カタログ
|
ダウンロード |
登録
for full access to applicationlibrary, spare parts catalog and newletters
お問合せ
お問合せ
私たちのニュース
NEW PRODUCT: PCTPro E&E
A fully automated Sievert instrument for measuring Gas (CO2, CH4, C2H6, N2) Sorption properties of materials.
See MoreCO2 CAPTURE & SEQUESTRATION
Find out our instrumentation is used to study CO2 Capture and Sequestration
See MoreOXIDATION BY CHEMILUMINESCENCE
NEW distribution agreement of ACL's Chemiluminescence systems for the analysis of oxidative reactions
See more
会議・展示会
- November 03, 2010 - November 03, 2010

- October 18, 2010 - October 22, 2010
MATERIAUX 2010
Nantes, FRANCE
Co-organized by more twenty learned societies, these events have been meeting opportunities between the national actors in the various fields of Materials Science.
For this 3rd edition, 14 symposiums are proposed whose:
- Civil engineering and Futur Habitat
- Energy Storage & Conversion
- Materials for Transport
- Materials & Environment
- Nanochemistry, Nanomatérials, Nanostructures
- Materials and Health Safety
- Thermodynamics and Materials for High Temperatures
- Mechanical properties and Spoiling
- Material stakes for the nuclear reactor (generation IV) - September 05, 2010 - September 10, 2010
SCTE 2010
Annecy, FRANCE
17th International Conference on Solid Compounds of Transition Elements
SCTE 2010 will be held in Annecy September, 5-10, 2010. The conference will be jointly organized by Institut Néel, CNRS-Université Joseph Fourier, Grenoble and Institut de Chimie de la Matière Condensée de Bordeaux, CNRS- Université Bordeaux 1, Bordeaux.
便利なリンク